SUPERIORTOP
is a heavy-duty three component, 100% solids, structural
epoxy floor surfacing system that provides
wear-resistance and protection from damaging substances
such as acids, alkalis, oils, fats and solvents.
SUPERIORTOP also provides skid-resistance and corrosion
protection of new or old masonry substrates. SUPERIORTOP
may be sealed with a topcoat to improve abrasion
resistance, gloss retention and non-skid properties. |
|
Superior
Epoxy Primer 171
Mix 1 volume of part A with 1 volume of part B.
Mix thoroughly, being sure to scrape the sides and bottom
with a strong mixing stick or a slow speed drill with a
paint propeller attachment. DO NOT mix more than can be
applied in 20 minutes. Apply mixed material by brush,
roller or squeegee at 150 to 200 square feet per gallon
(8-10 mils). The coverage will depend on the texture of
the surface. Apply toppings before primer becomes
tack-free, approximately 2-3 hours at 72°F.
Mortar
Mix thoroughly 2 parts by volume of part A and 1 part by
volume of part B of Superior Liquid Binder. Prepare the
mortar by adding 3-3 1/2 gallons of clean, dry sand to
each gallon of epoxy mix. Preferred types of sand are:
hard, high-grade silica sands such as Ottawa Flintshot,
Mission or their equivalents. Emery or other forms of
Alumina, and Silicon Carbide. If a blend of sand is used,
mix the sands together prior to adding to the epoxy. Blend
the epoxy and sand until the sand is thoroughly wet.
Screed the mortar out onto the previously primed area,
rake it to distribute, then compact and trowel to finish.
Blending may be accomplished by using a heavy duty, slow
speed 1/2" electric drill with a paddle, a Kol mixer or a
mortar pan and concrete
hoe.
SuperiorTop-S
To apply the topcoat of
Superior Gloss or
Superior Coat
over the SuperiorTop mortar overlay: stir each component
separately. Clear: Mix 2 volumes of part A with one volume
of part B. Pigmented: Mix 1 volume of part A with 1 volume
of part B. Mix thoroughly, being sure to scrape the sides
and bottom, with a strong mixing stick or slow-speed drill
equipped with a paint propeller. DO NOT mix more than can
be applied in 30 minutes. As a coating, apply mixed
material by brush or roller. For best results, two coats
should be applied. Allow the first coat to cure overnight.
Apply the second coat within 24 hours. If more time than
24 hours has elapsed, a light sanding of the first coat is
required. Superior Gloss can be placed as thick as desired
on horizontal surfaces without affecting the cure.
Skid-Proofing
When skid proofing is required, broadcast sand, emery or carborundum into the first coat while still tacky. Apply
the second coat to seal.
*** When
chemical-resistance is needed substitute
Superior Novalac
for Superior Gloss *** |